Polimeros (Material de Alto REndimiento)

Lapox ARA-32 | AH-732

Mixing ratio (Parts by weight) : 100 : 45 | Mix viscosity @ 25oC (mPa s) : Thixotropic paste | Pot life @ 25oC (minutes) : 25 – 35 | Glass transition temperature (Tg) (oC) : 75 – 85


Recommendations: An adhesive for secondary bonding of FRP to FRP on vertical surfaces without sagging even at elevated temperatures.