Lapox ARL-125 | AH-335

Mixing ratio (Parts by weight) : 100 : 32 | Mix viscosity @ 25oC (mPa s) : 300 – 700 | Pot life @ 25oC (minutes) : 50 – 60 | Glass transition temperature (Tg) (oC) : 75 – 85


Recommendations: A medium viscosity epoxy system with moderate pot life recommended for Resin Transfer Moulding (RTM), Resin Infusion (RI) and hand lay-up for making small to large composite components.