Lapox ARL-125 | AH-367 GL

Mixing ratio (Parts by weight) : 100 : 32 | Mix viscosity @ 25oC (mPa s) : 200 – 300 | Pot life @ 25oC (minutes) : 300 – 380 | Glass transition temperature (Tg) (oC) : 75 – 85


Recommendations: A GL certified low viscosity epoxy system recommended for Resin Infusion (RI), Resin Transfer Moulding (RTM), pultrusion, filament winding, hand lay-up lamination, vacuum and pressure bag techniques.