Mixing ratio (Parts by weight) : 100 : 32 | Mix viscosity @ 25oC (mPa s) : 1,500 – 2,500 | Pot life @ 25oC (minutes) : 300 – 350 | Glass transition temperature (Tg) (oC) : 130 – 140


Recommendations: An ambient curing epoxy system offers a long pot life with high Tg.