Mixing ratio (Parts by weight) : 100 : 32 | Mix viscosity @ 25oC (mPa s) : 700 – 1,200 | Pot life @ 25oC (minutes) : 14 – 20 | Glass transition temperature (Tg) (oC) : 80 – 90


Recommendations: A medium viscosity epoxy system with short pot life recommended for Resin Transfer Moulding (RTM) and hand lay-up for making small to large composite components.