Polimeros (Material de Alto REndimiento)

Lapox ARL-135 LV | AH-337

Mix viscosity @ 25oC : 200 – 300 | Pot life @ 25oC (minutes) : 300 – 380 | Glass transition temperature (Tg) (oC) : 75 – 85


Recommendations: A low viscosity epoxy system with long pot life recommended for filament winding, Resin Transfer Moulding (RTM) and Resin Infusion (RI) processes for making small to large components, including wind turbine blades.