Lapox ARL-135LV | AH-411

Mixing ratio (Parts by weight) : 100 : 24 | Mix viscosity @ 25oC (mPa s) : 250 – 400 | Pot life @ 25oC (minutes) : 90 – 120 | Glass transition temperature (Tg) (oC) : 125 – 135


Recommendations: A very low viscosity epoxy system for high Tg. The product is recommended for Resin Infusion (RI), hand lay-up and tooling applications.