Mixing ratio (Parts by weight) : 100 : 90 | Mix viscosity @ 25oC (mPa s) : 300 – 600 | Pot life @ 25oC (minutes) : > 8 | Glass transition temperature (Tg) (oC) : 115 – 125


Recommendations: A hot curing epoxy system offers superior fiber wetting property giving higher productivity. Optimum curing delivers excellent mechanical and electrical properties with good surface finish.