Lapox L-12 | K-5200

Mixing ratio (Parts by weight) : 100 : 24 | Mix viscosity @ 25oC (m Pas) : 4,000 – 6,000 | Pot life @ 25oC (days) : 2 – 3 | Glass transition temperature (Tg) (oC) : 180 – 190


Recommendations: A hot curing epoxy system offers a long pot life and very high Tg.