Lapox L-12 / AH-113 / K-13

Mixing ratio (Parts by weight) : 100 : 95 : 0.5-2.0 | Mix viscosity @ 25oC (mPa s) : 1,900 – 2,100 | Pot life @ 25oC (minutes) : > 8 | Glass transition temperature (Tg) (oC) : 165 – 185


Recommendations: A low viscosity, hot curing epoxy system for pultrusion and filament winding in electro composite manufacturing.