Mixing ratio (Parts by weight) : 100 : 6 | Mix viscosity @ 25oC (mPa s) : Paste (grey) | Pot life @ 25oC (minutes) : 15 – 20 | Glass transition temperature (Tg) (oC) : 85 – 95


Recommendations: A gel coat with high thermal conductivity, excellent hardness and surface finish.