Mixing ratio (Parts by weight) : 100 : 30 | Mix viscosity @ 25oC (mPa s) : 400 – 600 | Pot life @ 25oC (minutes) : 120 – 180 | Glass transition temperature (Tg) (oC) : 130 – 140


Recommendations: A standard tooling system with excellent Tg. The product is suitable to make tools with hand lay-up and infusion processes of varying sizes.