Polymers Performance Materials

Lapox ARL-140 | AH-419

Mixing ratio (Parts by weight) : 100 : 42 | Mix viscosity @ 25oC (mPa s) : 2,500 – 3,000 | Pot life @ 25oC (minutes) : 600 – 700 | Glass transition temperature (Tg) (oC) : 190 – 220


Recommendations: A tooling system with high Tg for dimensional stability even at high temperatures.