Polymers Performance Materials

Lapox ARL-143 | AH-319

Mixing ratio (Parts by weight) : 100 : 15 | Mix viscosity @ 25oC (mPa s) : 3,500 – 5,000 | Pot life @ 25oC (minutes) : 20 – 25 | Glass transition temperature (Tg) (oC) : 95 – 105


Recommendations: A moderate viscosity modified epoxy system with short pot life to suit different processing techniques. The product is recommended for fire retardant applications.