Lapox ARPN-36 | K-86

Mixing ratio (Parts by weight) : 100 : 3-6 | Pot life @ 25oC (hours) : > 8 | Glass transition temperature (Tg) (oC) : 165 – 180


Recommendations: A hot curing epoxy system delivers stable B-stage prepregs with a very high Tg.