Polimeros (Material de Alto REndimiento)

Lapox ARL-135 LV | AH-422

Mixing ratio (Parts by weight) : 100 : 35 | Mix viscosity @ 25oC (mPa s) : 400 – 600 | Pot life @ 25oC (minutes) : 300 – 350 | Glass transition temperature (Tg) (oC) : 110 – 120


Recommendations: A medium viscosity epoxy system with long pot life and high Tg. The product is recommended for hand lay-up and Resin Infusion (RI) of large components.