Polimeros (Material de Alto REndimiento)

Lapox ARL-158 | AH-419

Mixing ratio (Parts by weight) : 100 : 42 | Mix viscosity @ 25oC (mPa s) : 300 – 500 | Pot life @ 25oC (minutes) : 600 – 700 | Glass transition temperature (Tg) (oC) : 170 – 200


Recommendations: A low viscosity epoxy system offers high Tg for dimensional stability even at high temperatures.