Lapox AH-338 | aliphatic amine; curing agent; composite; adhesive; coating

Colour (Gardner) : Max 4 | Viscosity @ 25oC (mPa s) : 10 – 50 | Pot life @ 25oC : 600 min – 700 hr

Posted in PO PM Product

Lapox AH-337 | aliphatic amine; curing agent; composite; adhesive; coating

Colour (Gardner) : Max 4 | Viscosity @ 25oC (mPa s) : 10 – 50 | Pot life @ 25oC : 300 min – 380 hr

Posted in PO PM Product

Lapox AH-336 | aliphatic amine; curing agent; composite; adhesive; coating

Colour (Gardner) : Max 4 | Viscosity @ 25oC (mPa s) : 20 – 100 | Pot life @ 25oC : 80 min – 100 hr

Posted in PO PM Product

Lapox AH-335 | aliphatic amine; curing agent; composite; adhesive; coating

Colour (Gardner) : Max 4 | Viscosity @ 25oC (mPa s) : 20 – 100 | Pot life @ 25oC : 50 min – 60 hr

Posted in PO PM Product

Lapox AH-334 | aliphatic amine; curing agent; composite; adhesive; coating

Colour (Gardner) : Max 4 | Viscosity @ 25oC (mPa s) : 50 – 150 | Pot life @ 25oC : 25 min – 35 hr | Mixing ratio (Parts by weight) : 32

Posted in PO PM Product

Lapox AH-333 | aliphatic amine; curing agent; composite; adhesive; coating

Colour (Gardner) : Max 4 | Viscosity @ 25oC (mPa s) : 150-300 | Pot life @ 25oC : 14 min – 20 hr

Posted in PO PM Product

Lapox AH-332 | aliphatic amine; curing agent; composite; adhesive; coating

Colour (Gardner) : Max 4 | Viscosity @ 25oC (mPa s) : 10 – 150 | Pot life @ 25oC : 10 min – 10 hr | Mixing ratio (Parts by weight) : 32

Posted in PO PM Product

Lapox AH-311 | aliphatic amine; curing agent; composite; adhesive; coating

Colour (Gardner) : Max 4 | Viscosity @ 25oC (mPa s) : 10 – 150 | Pot life @ 25oC : 10 min – 10 hr | Mixing ratio (Parts by weight) : 32

Posted in PO PM Product